Effect of Na2CO3 and CaCO3 on Coreduction Roasting of Blast Furnace Dust and High-phosphorus Oolitic Hematite

查看全文 作  者:[1]曹允业;[1]孙体昌;KOU [1]Jue;XU [1]Chengyan;GAO [1]Enxia 高影响力作者 机构地区:[1]School of Civil & Environmental Engineering, Key Laboratory of High-Efficient Mining and Safety of Metal Mines, Ministry of Education University of Science and Technology Beijing, Beijing 100083, China高影响力机构 出  处:《Journal of Wuhan University of Technology(Materials Science)》索引2017年第32卷第3期,共8页高影响力期刊 基  金:Funded by National Natural Science Foundation of China(No.51134002) 摘  要:Iron was recovered from blast furnace dust and high-phosphorus oolitic hematite in the presence of Na_2CO_3 and CaCO_3 additives. The functions of Na_2CO_3 and CaCO_3 during the coreduction roasting process were investigated by XRD and SEM-EDS analyses. Results indicate that these additives not only hinder the reduction of fluorapatite, CaCO_3 also decreases the P content of direct reduced iron(DRI) by increasing the reduction alkalinity. P remains as fluorapatite in the slag, which can be removed by grinding and magnetic separation under optimal conditions. The Na_2CO_3 promotes hematite reduction and improves the iron recovery(εFe) by replacing the FeO from fayalite, which results in quick growth and aggregation of metallic iron and improvement of ε_(Fe) in DRI. A DRI with 91.88 mass% Fe, and 0.065 mass% P can be achieved at a recovery of 87.86 mass% under the optimal condition. 关 键 词:鲕状赤铁矿 高炉粉尘 焙烧过程 碳酸钙 共还原 碳酸钠 高磷 SEM-EDS
相关文献

参考文献(18)

引证文献(4)

耦合文献(138)

网站首页 | 关于我们 | 联系我们 | 产品服务 | 客服中心 | 广告服务 | 版权声明 | 网站联盟 | 友情链接 | 售卡网点

版权所有© 渝B2-20050021-1 渝公网安备 50019002500403号 违法和不良信息举报中心

互联网出版许可证 新出网证(渝)字10号 全国400电话 - 免长途话费