| 1 | 血浆游离DNA水平增高可作为预测重型颅脑损伤患者死亡率的独立指标(英文)显示文摘Trauma is the leading cause of death under 45 years worldwide and up to 50% of trauma fatalities are due to brain injury.Prediction of outcome is one of the major problems associated with severe TBI and research efforts have focused on the investigation of biomarkers with prognostic value following TBI. Therefore,our aim was to investigate whether cell-free DNA concentrations correlated to short-term primary outcome( survivor or death) and GCS scores following severe TBI. A total of 188 victims of severe TBI were enrolled in this prospective study,outcome variables comprised: survival and neurological assessment using the GCS at ICU discharge. Control blood samples were obtained from 25 healthy volunteers. Peripheral venous blood was collected at admission in the ICU. Plasma DNA was measured using a real-time quantitative PCR assay for the β-globin gene. There was correlation between higher DNA levels and both fatal outcome and lower hospital admission GCS scores. Plasma DNA concentrations at the chosen cut- off point( ≥171,381 kilogenomesequivalents /L) predicted mortality with a specificity of 90% and a sensitivity of 43%. Logistic regression analysis showed that elevated plasma DNA levels were independently associated with death( P < 0. 001). In conclusion,high cell-free DNA concentration was a predictor of short-term mortality following severe TBI. | Rodrigues Filho EM1 Simon D Ikuta N Klovan C Dannebrock F de Oliveira CO Regner A | 2014 | 中华神经外科疾病研究杂志2014,13,3: | 6 |
| 2 | Cy clability and dissolution of manganese i n substituted stoichiometric and non-sto ichiometric lithium manganese oxides at high temperature 显示文摘 | IKUTA H WAKIHARA M | 2000 | Electrochemistry2000,68,6: | 1 |
| 3 | Spinel phases LiAlyMn2-yO4(y=0,1/12,1/9,1/6,1/3) and Li(Al,M)1/6Mn11/6O4(M = Cr,Co) as the cathode for rechargeable lithium batteries显示文摘 | Song D Ikuta H Uchida T | 1999 | Solid State Ionics1999,117,12: | 1 |
| 4 | The spinel phases LiAly Mn2-y O4 ( y = 0, 1/12,1/9,1/6,1/3 ) and Li ( A1, M) (1/6) Mn11/6 O4 ( M = Cr, Co) as the cathode for rechargeable lithium batteries 显示文摘 | Song D Ikuta H Uchida T | 1999 | Solid State Ionics1999,117,12: | 1 |
| 5 | The Spinel Phases LiAlyMn2-yO4 (y=0,1/12,1/9,1/6,1/3) and Li(Al,M)1/6Mn11/6O4(M=Cr,Co) as the Cathode for Rechargeable Lithium Batteries显示文摘 | Ikuta H Uchida T | 1999 | Solid State Ionics1999,117,12: | 1 |
| 6 | The spinel phases LiAlyMn2-yO4(y=0,1/12,1/6,1/3) and Li(Al,M)1/6Mn11/6O4(M=Cr,Co) as the cathode for rechargeable lithium batteries显示文摘 | SONG D IKUTA H UCHIDA T | 1999 | Solid State Ionics1999,117,2: | 1 |
| 7 | The spinel phases LiAlyMn2 _yO4 ( y = 0,1/12, 1/9,1/6,1/3) and Li(A1,M)1/6Mn11/6O4(M=Cr,Co) as the cathode for rechargeable Lithium batteries 显示文摘 | Song D Ikuta H | 1999 | Solid State lonics1999,117,: | 1 |
| 8 | 显示文摘 | Song D Ikuta H Uchida T | 1999 | Solid State Ionics1999,117,: | 1 |
| 9 | Do fences protect birds from human disturbance? 显示文摘 | IKUTA L A BLUMSTEIN D T | 2003 | Biological Conservation2003,112,3: | 1 |
| 10 | The spinel phases Li AlyMn2=yO4 (y =0, 1/12,1/9, 1/6, 1/3)and Li(Al,M)1/6Mn1/6O4 (M = Cr, Co) as the cathode for reehargeable lithium batteries显示文摘 | Song D Ikuta H Uehida T | 1999 | Solid State Ionics1999,117,12: | 1 |
| 11 | The spinel phases LiAlyMn2-yO4(y=0,1/12,1/9,1/6,1/3) and Li(Al,M)1/6Mn11/6O4(M=Cr,Co) as the cathode for rechargeable lithium batteries显示文摘 | Song D Ikuta H Uchida T | | 0,,: | 1 |
| 12 | Amorphous MoS2 as the cathode of lithium secondary batteries显示文摘 | Miki Y Nakazato D Ikuta H | 1995 | J Power Sources1995,54,50: | 1 |
| 13 | The spinel phases LiAlyMn2-yO4(y = 0, 1/12, 1/9, 1/6, 1/3) and Li (Al, M)1/6Mn11/6O4 (M = Cr, Co) as the cathode for rechargeable lithium batteries 显示文摘 | Song D Ikuta H Uchida T | 1999 | Solid State Ionies1999,117,: | 1 |
| 14 | The amphioxus genome illuminates vertebrate origins and cephalochordate biology显示文摘 | Holland LZ Albalat R Azumi K Benito-Gutiérrez è Blow MJ Bronner-Fraser M Brunet F Butts T Candiani S Dishaw LJ Ferrier DEK Garcia-Fernàndez J Gibson-Brown JJ Gissi C Godzik A Hallb(o)(o)k F Hirose D Hosomichi K Ikuta T Inoko H Kasahara M Kasamatsu J Kawas | | 0,,07: | 1 |
| 15 | The spinel phases LiAlMn2-xO4(Y=0, 1/12, 1/9, 1/6, 1/3)and Li (Al, M)1/6n111/6O4(M=Cr,Co)as the cathode for rechargeable lithium batteries显示文摘 | Ikuta H Uchida T | 1999 | Solid State Ionics1999,,117: | 1 |
| 16 | The spinel phases LiAlyMn2-yO4(y=0, 1/12, 1/9, 1/6, 1/3) and Li(Al, M)1/6Mn11/6O4 (M=Cr, Co) as the cathode for rechargeable lithium batteries显示文摘 | Song D Ikuta H Uchida T | 1999 | Solid State Ionics1999,117,12: | 1 |
| 17 | Joining of cast iron used self-fluxing alloy coating显示文摘 | Yara H Ikuta A Fujiki D | 1993 | Quarterly Journal of the Japan Welding Society1993,11,4: | 1 |
| 18 | Precise ben- ding angle control of hydraulic active catheter by pressure pulse drive 显示文摘 | IKUTA K MATSUDA Y YAJIMA D | 2010 | IEEE International Conference on Robot- ics and Automation2010,,: | 1 |
| 19 | 显示文摘 | Song D Ikuta H Uchida T | 1999 | Solid State Ionics1999,117,: | 1 |
| 20 | The spinel phase Li-AlyMn2-yO4 (y=0,1/12,1/9,1/6,1/3)and Li(A1,M)1/6Mn11/6O4 (M=Cr,Co) as cathode for rechargeable lithium batteries显示文摘 | SONG D IKUTA H WAKIHARA M | 1999 | Solid State Ionics1999,117,: | 1 |