Revisiting the thermal ageing on the metallised polypropylene film capacitor:from device to dielectric film

查看全文 作  者:Yushuang [1]He;Feipeng [1]Wang;Guoqiang [1]Du;Lei [1]Pan;Kaizheng [2]Wang;Reimund [3]Gerhard;Ronald [4]Plath;Pawel [5]Rozga;Pavel [6]Trnka 高影响力作者 机构地区:[1]State Key Laboratory of Power Transmission Equipment and System Security and New Technology,Chongqing University,Chongqing,China;[2]Faculty of Electrical Engineering,Kunming University of Science and Technology,Kunming,China;[3]Soft Transducer Materials and Systems,Universität Potsdam,Potsdam,Germany;[4]Faculty IV Electrical Engineering and Computer Science,Technische Universität Berlin,Berlin,Germany;[5]Institute of Electrical Power Engineering,Lodz University of Technology,Lodz,Poland;[6]Faculty of Electrical Engineering,University of West Bohemia,Pilsen,Czech Republic高影响力机构 出  处:《High Voltage》索引2023年第8卷第2期,共10页高影响力期刊 基  金:Major Research Plan of the National Natural Science Foundation of China,Grant/Award Number:92166206;Fundamental Research Funds for the Central Universities,Grant/Award Number:2022CDJQY-014;Ministry of Education of China through the 111 project,Grant/Award Number:BP0820005。 摘  要:Metallised polypropylene film capacitors(MPPFCs)are widely used in power electronics and are generally degraded by elevated temperatures.This work aims to determine the relationships between the structural changes of MPPFC and the microstructural variations of the PP film during the thermal ageing of MPPFC at 100℃ for 38 days.The capacitance of MPPFC has a slight decrease during thermal ageing.However,the breakdown voltage of the MPPFC decreases by 39.4%by the ageing.The partial discharge(PD)number of MPPFC increases linearly with ageing time.The tear-down analysis of the MPPFC reveals that the molecular structure of the PP film has not been altered but has led to molecular chain scission and the generation of some polar fragments/groups.Meanwhile,the relative permittivity of the PP films rises as the ageing time increases.Moreover,thermal ageing causes the conversion of aluminum to alumina in the metallised electrode,which is hydrophilic for polar groups and leads to an adhesion effect between the metallised electrodes and the PP film.Contact angle measurements prove that the surface hydrophilicity of the PP sample increased after thermal ageing.Therefore,the PD/breakdown voltage in the MPPFC increases/decreases due to the uneven adhesion of the metallised PP film. 关 键 词:FILM THERMAL ageing
相关文献

参考文献(32)

引证文献(12)

网站首页 | 关于我们 | 联系我们 | 产品服务 | 客服中心 | 广告服务 | 版权声明 | 网站联盟 | 友情链接 | 售卡网点

版权所有© 渝B2-20050021-1 渝公网安备 50019002500403号 违法和不良信息举报中心

互联网出版许可证 新出网证(渝)字10号 全国400电话 - 免长途话费